[Date Prev][Date Next][Thread Prev][Thread Next][Date Index][Thread Index]
Re: arsclist creating sticky shed deterioration
It goes back before 1975. Del supplied a list of 3M product numbers which
went "bad." I've listed these is paragraph form on my "Sticky tape" page on
my website, www.soundsaver.com.
Steve Smolian
----- Original Message -----
From: Parker Dinkins <parker@xxxxxxxxxxxxxxxxx>
To: <ARSCLIST@xxxxxxxxxxxxxxxx>
Sent: Monday, May 14, 2001 5:47 PM
Subject: Re: arsclist creating sticky shed deterioration
> on 5/14/01 3:44 PM, Sarah Stauderman wrote:
>
> We had extensive conversations with Delos Eilers and Bill Lund at 3M's
Audio
> Video Technology Lab several years ago on this issue.
>
> It was their feeling at the time that the mere presence of moisture did
> nothing to hasten the onset of the sticky shed syndrome, but instead it
was
> caused by the breakdown over time of long chain polymers/molecules which
> invited water/moisture to occupy spaces otherwise not available.
>
> Mr. Eilers was kind enough to give me a copy of the notes of the speech he
> gave on this topic at an AES meeting. These notes documented his
recommended
> times and temperatures for re-curing the binder compound by baking.
>
> It's important to keep remember that tapes can have many different
problems.
> In discussing sticky shed syndrome, you're talking about a specific
problem
> with open reel analog audio tapes manufactured largely in the US between
> 1975 and 1985.
>
> Later.
>
> Parker
>
> Also: http://www.masterdigital.com/24bit/analogtape.html#anchor1163399
>
> >> Do you think if I leave a reel of 1981
> >> vintage 456 in my bathroom for a month of showers it will be hydrolized
> >> enough?
> >
> > This has been part of the problem for studying tape deterioration: as
far as
> > I know, no one has been able to create "sticky shed" in the lab. It
makes it
> > really tough to determine what physical mechanism causes deterioration.
> >
> > As far as the weight and thickness of Pellon (other brand names are
Hollytex
> > and Reemay), I believe that the one used for our experiment was 4 mil
(thin).
> >
> > Sarah Stauderman
>
>
> ---
> Parker Dinkins CD Mastering + Audio Restoration
> MasterDigital Corporation http://www.masterdigital.com
>
>
> -
> For subscription instructions, see the ARSC home page
> http://www.arsc-audio.org/arsclist.html
> Copyright of individual posting is owned by the author of the posting and
> permission to re-transmit or publish a post must be secured
> from the author of the post.
>
>